TPU & Nylon Injection Molding | TOPSEALS Custom Seals

TPU & Nylon Injection Molding | TOPSEALS Custom Seals

TPU & Nylon Injection Molding

TOPSEALS manufactures precision injection molded TPU and Nylon (PA6 / PA66, glass-filled PA) parts for mechanical, design and OEM engineers across hydraulic fluid power, automotive, industrial robotics and chemical equipment. TPU and Nylon are hygroscopic engineering polymers with unique molding challenges: moisture degradation, variable shrinkage, post-mold dimensional shift, fiber orientation warpage and poor surface quality. Our factory has optimized injection molding workflows, mold design, material drying and process parameters for both rigid Nylon and flexible TPU, resolving common production defects including splay marks, bubbles, sink marks, warpage, brittleness, flash and incomplete filling.

Core Defects & Pain Points

Most molding failures for TPU and Nylon originate from material hygroscopic behaviour and anisotropic shrinkage, not simple machine parameter tuning:

  • Moisture induced splay, bubbles & polymer chain degradation. Nylon and TPU rapidly absorb ambient moisture. If not fully dried, water vaporizes inside the barrel during injection, creating silver streaks, internal voids and reduced mechanical strength.
  • Warpage & post-mold dimensional drift. Nylon shows high volumetric shrinkage; glass-filled grades have directional shrinkage from fiber alignment. Nylon also continues to swell after molding as it absorbs ambient moisture, shifting dimensions weeks after production.
  • Sink marks & internal voids. Thick sections, heavy ribs and boss areas trap material shrinkage. Insufficient holding pressure creates surface depressions and hidden internal voids.
  • TPU sticking, flash and poor release. Flexible TPU has high surface adhesion. Insufficient draft angle, poor mold polishing or excessive injection pressure causes parts to stick in cavities, tearing or flash along parting lines.
  • Overmolding adhesion failure (TPU on Nylon). Poor surface energy, contaminated substrate or mismatched melt temperature creates weak bonding and delamination under cyclic load.

TOPSEALS Injection Molding Process

1. Material Pre-Drying & Raw Material Validation

We use dehumidifying hopper dryers with controlled dew point. Nylon PA6/PA66 dried at 80-100°C for 4-6 hours to reduce moisture below 0.2%. TPU dried at 80-110°C for 2-4 hours to target moisture <0.02%. Material moisture content is verified before every molding run.

2. Mold Design & Mold Flow Simulation

We run mold flow analysis before mold machining to predict filling pattern, fiber orientation, cooling rate and shrinkage. Gates are positioned at thick sections to reduce sink marks. For TPU molds, we increase draft angle (2-3° recommended) and polish mold surfaces to reduce sticking risk.

3. Injection, Packing & Cooling Parameter Tuning

Nylon: Melt temperature 240-280°C; mold temperature 80-100°C. Controlled holding pressure compensates high volumetric shrinkage. Lower injection speed for glass-filled grades reduces fiber breakage.
TPU: Melt temperature 185-225°C; mold temperature 30-50°C. Longer cooling cycle to prevent deformation at ejection. Avoid excessive barrel residence time to prevent thermal degradation and yellowing.

4. Ejection, Post-Mold Conditioning & Secondary Operations

Nylon parts are stabilized after molding. For functional precision components, we perform moisture conditioning under controlled RH to simulate end-use environment. Secondary services include overmolding, hot stamping, assembly and custom surface finishing.

5. Dimensional & Mechanical Quality Inspection

All finished components are inspected under controlled temperature. For Nylon, we distinguish dry-state dimensions vs conditioned moisture dimensions for your drawing tolerance. Inspection reports are available for OEM projects.

Material Selection & Application Reference

  • Nylon PA6 / PA66 (Unfilled): High toughness, good wear resistance. Hydraulic wear guides, bushings, structural spacers.
  • Glass-filled Nylon (GF10, GF20, GF30): Higher stiffness, lower shrinkage, improved heat resistance. Automotive structural parts, pump housings, valve components.
  • TPU (Thermoplastic Polyurethane): Flexible, excellent abrasion resistance, high tear strength. Hydraulic & pneumatic seals, gaskets, shock absorbers, overmolded soft-touch layers.

DFM Design Guidelines

  • Maintain uniform wall thickness; avoid abrupt thickness transitions which cause sink marks and warpage.
  • Add generous radii to all internal corners to reduce stress concentration and improve melt flow.
  • For TPU parts, use minimum draft angle of 2°; avoid sharp undercuts without side action mold design.
  • For glass-filled Nylon, align gate direction to minimise fiber orientation warpage.
  • Specify whether Nylon dimensions are measured at dry or conditioned moisture state.
  • Design gates at thickest wall sections to allow holding pressure to eliminate voids and sink marks.

Industries Served

  • Hydraulic & Pneumatic Systems: TPU seals, wear rings, nylon guide bushes, back-up rings, valve components
  • Automotive & Motorcycle: Nylon structural brackets, TPU shock pads, sensor holders, cable guides
  • Robotics & Automation: Nylon wear inserts, TPU vibration dampers, lightweight support components
  • Fluid & Chemical Equipment: Nylon pump housings, TPU corrosion resistant sealing elements

FAQ

Why do nylon parts change size weeks after injection molding?

Nylon is hygroscopic. After molding, it absorbs moisture from air and swells. We recommend conditioning parts to target RH before final dimensional inspection for precision applications.

Can TPU be overmolded directly onto Nylon substrates?

Yes, but surface preparation, substrate temperature and material grade matching are critical. Poor surface energy or contamination will cause delamination.

What is the typical tolerance for injection molded TPU and Nylon parts?

Rigid unfilled Nylon ±0.05~0.10 mm; glass-filled nylon ±0.03~0.08 mm. Flexible TPU has wider tolerance ±0.10~0.20 mm due to elasticity.

Explore Other Manufacturing Processes

Request Free DFM Mold Flow Review & Quotation

Send your CAD drawings, material grade, hardness requirement and operating environment details. We will run DFM analysis, identify risks of warpage, sink marks or delamination, and provide formal quotation before mold manufacturing.

Contact us